Capable Classification Society Quality Authentication from LR, ABS, NK, GL, DNV, BV, KR, RINA, CCS,DH36 shipbuilding steel plate is used for shipbuiling&platform.The shipbuilding steel plate grade DH36 is the high tensile strength steel.DH36 shipbuilding steel is the Hull structural steel,with it’s good toughness properties, higher strength,strong corrosion-resistance,the processing properties,and welding properties.ASTM A131 DH36 steel plate can be used in the manufacture of the ship’s hull structure whose weight is more than 10000 tons.
ABS DH36 Shipbuilding Steel Specification:Thickness: 4mm to 260mm,
Width: 1200mm to 4000mm
Length: 3000mm to 18000mm. ABS DH36 Shipbuilding Steel Application:
ABS DH36 Shipbuilding steel plates are mainly used for making the offshore oil drilling platform, the hull of ship building and ship repairing, the platform pipe joints and other components.
Grade | C max | Si max | Mn | P max | S max | Als min | Ti max | Cu max | Cr max | Ni max | Mo max | Nb | V |
DH36 | 0.18 | 0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 | 0.02-0.05 | 0.05-0.10 |
Note: Generally speaking CE will be ≤ 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.38% (thickness ≤ 50mm),≤0.40%( when the thickness >50-100). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.
Grade | Rm (MPa) | Re(MPa) min | A% min | Akv/J min | |
DH36 | 490-630 | 355 | 21 | E.T °C | Thickness (mm) |
-20 | ≤ 50 | >50-70 | >70-100 | ||
L | C | L | C | L | C |
34 | 24 | 41 | 27 | 50 | 34 |
Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.
DH36 steel plate Condition Of Delivery
Grade | Fine grains elements | category | The thickness of steel | ||
≤ 12 | >12.5-20 | >20-25 | >25-35 | >35-50 | >50-100 |
DH36 | Nb+V or V | Plate/ sheet | A(50) | N(50),CR(50),TM(50) | N(50),CR(25),TM(50) |
Profile steel | N(50),CR(50),TM(50),AR*(25) | – | |||
Al or Al+Ti | Plate/ sheet | A(50) | AR*(25) | – | |
N(50),CR(50),TM(50) | N(50),CR(25),TM(50) | ||||
Profile steel | A(50) | N(50),CR(50),TM(50),AR*(25) | – |
2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.
DH36 steel plate Contrast in the different standard
ASTM A131M | TOCT 5521 | BS LR | GB712 |
DH36 | D36 | DH36 | D36 |
DH36 steel plate Available Specification
variety | Thickness (mm) | Width (mm) | Longth/ inner diameter (mm) | |
Shipbuilidng plate | cutting edges | 6~200 | 1500~3000 | 3000~15000 |
non- cutting edges | 1300~3000 | |||
Shipbuilidng coil | cutting edges | 1.2~19 | 1500~2000 | 760+20~760-70 |
non-cutting edges | 1510~2010 |
Thickness (mm) | theoretical weight | Thickness (mm) | theoretical weight | ||
Kg/ft2 | Kg/m2 | Kg/ ft2 | Kg/m2 | ||
6 | 4.376 | 47.10 | 25 | 18.962 | 196.25 |
7 | 5.105 | 54.95 | 26 | 20.420 | 204.10 |
8 | 5.834 | 62.80 | 28 | 21.879 | 219.80 |
10 | 7.293 | 78.50 | 30 | 23.337 | 235.50 |
11 | 8.751 | 86.35 | 32 | 25.525 | 251.20 |
12 | 10.21 | 94.20 | 34 | 26.254 | 266.90 |
14 | 10.939 | 109.90 | 35 | 27.713 | 274.75 |
16 | 11.669 | 125.60 | 40 | 29.172 | 314.00 |
18 | 13.127 | 141.30 | 45 | 32.818 | 353.25 |
20 | 14.586 | 157.00 | 48 | 35.006 | 376.80 |
22 | 16.044 | 172.70 | 50 | 36.464 | 392.50 |
24 | 18.232 | 188.40 |
nominal thickness(mm) | The thickness deviation with following width (mm) | |||
≤1200 | >1200~1500 | >1500~1800 | >1800 | |
>6.0~8.0 | ±0.29 | ±0.30 | ±0.31 | ±0.35 |
>8.0~10.0 | ±0.32 | ±0.33 | ±0.34 | ±0.35 |
>10.0~12.0 | ±0.35 | ±0.36 | ±0.37 | ±0.43 |
nominal thickness(mm) | minus deviation (mm) | The thickness deviation with following width (mm) | |||||||||
> 1000 ~1200 | > 1200 ~1500 | > 1500 ~1700 | > 1700 ~1800 | > 1800 ~2000 | > 2000 ~2300 | > 2300 ~2500 | > 2500 ~2600 | 2600 ~2800 | > 2800 ~3000 | ||
>12~25 | -0.8 | +0.2 | +0.2 | +0.3 | +0.4 | +0.6 | +0.8 | +0.8 | +1.0 | +1.1 | +1.2 |
>25~30 | -0.9 | +0.2 | +0.2 | +0.3 | +0.4 | +0.6 | +0.8 | +0.9 | +1.0 | +1.1 | +1.2 |
>30~34 | -1.0 | +0.2 | +0.3 | +0.3 | +0.4 | +0.6 | +0.8 | +0.9 | +1.0 | +1.2 | +1.3 |
>34~40 | -1.1 | +0.3 | +0.4 | +0.5 | +0.6 | +0.7 | +0.9 | +1.0 | +1.1 | +1.3 | +1.4 |
>40~45 | -1.2 | +0.4 | +0.5 | +0.6 | +0.7 | +0.8 | +1.0 | +1.1 | +1.2 | +1.4 | +1.5 |