4047 (BAlSi-4) Aluminum

4047 aluminum is a 4000-series aluminum alloy. The main alloying addition is silicon. Cited properties are appropriate for the as-fabricated (no temper or treatment) condition. 4047 is the Aluminum Association (AA) designation for this material. In European standards, it will be given as EN AW-4047. BAlSi-4 is the AWS designation. Additionally, the UNS number is A94047.

It originally received its standard designation in 1964.

Similar Alloys

Category:
4047 aluminum (also known as alloy 4047 and AL4047) is an aluminum silicon brazing or filler alloy with good corrosion resistance. The main difference between alloy 4047 and it’s AL4043 counterpart is its higher silicon content. With 11-13% silicon, AL 4047 is generally used when high fluidity and reduced shrinkage and hot cracking is needed for specific repairs or manufacturing. Additionally, 4047 is suitable at elevated temperatures making it particularly useful in the automotive industry for parts and engine blocks. Other applications include welding filler wires, leak tight joints, housing requirements, window frames, liners such as laser welded covers for microwave integrated circuits, and other similar devices.

4047 is one of 4000 series alloys. 4 series aluminum alloys are aluminum alloys with silicon as the main alloying element. Most of the alloys are heat-treated non-strengthable aluminum alloys, which refer to alloys containing Cu, Mg, and Ni, as well as welding heat treatment strengthening After the alloy has absorbed certain elements, it may be strengthened by heat treatment. Because of the high silicon content, low melting point, good melt fluidity, and the final product will not be brittle, this series of alloys are mainly used to make aluminum alloy welding additives, such as brazing plates, welding rods and welding wires. In addition, due to the high wear resistance and high temperature resistance of some of this series of alloys, they are also used to make pistons and heat-resistant parts. The alloy containing about 5% of silicon is black-gray after anodizing and coloring, so it is used as building materials and manufacturing decorative parts.

4047 alloy aluminium is a non-heat treatable wrought alloy type with good corrosion resistance. It is a filler alloy, and is quite similar to aluminium / aluminum 4043 except for the higher silicon content in 4047 aluminum alloy. The higher silicon content provides improved fluidity during welding process with smooth finishes, as well as reduced shrinkage. It is suitable for elevated temperature operations.

Physical Properties:

PropertiesMetricImperial
Density2.6 g/cm30.096 lb/in3

Typical Parameters:

Wire diameterRangeBase material thicknessSuggestedWire feedGas flowConsumption
100 ft of weld
INCHESAMPSVOLTSINCHESAMPSVOLTSIPMCFHPOUNDS
0.03060-17013-240.0629022260251.5
0.094110233201.8
0.125130233802
0.187150244304
0.250175245106
0.03570-18015-260.0629023250351.5
0.125130243602
0.250170254706
0.047140-26020-290.09411025215451.8
0.125150262902
0.250190263706
0.3752202743016
0.062190-35025-300.25020026190556
0.3752302721516
0.5002602824030
0.7502802926150
1.00030030280105
0.094280-40026-310.500280281706530
0.7502902917550
>1.00030030180150+

Applications:

  • Laser welded covers for microwave integrated circuits
  • Housing
  • Welding filler wires
  • Liners
  • Leak-tight joints