17-4 PH Stainless Steel(Precipitation Hardening)

17-4PH alloy is composed of copper, niobium precipitation, hardening, martensitic stainless steel. Features: After heat treatment, the mechanical properties of the product are improved and compressive strength up to 1100-1300 MPa (160-190 ksi) can be achieved. This grade can not be used at temperatures above 300 ° C (572 ° F) or very low temperatures. It has good corrosion resistance to atmospheric and dilute acids or salts, and its corrosion resistance is the same as 304 and 430. 17-4PH is a martensitic precipitation hardened stainless steel .17-4PH performance characteristics is easy to adjust the strength level, you can change the heat treatment process to be adjusted.Martensite transformation and aging treatment to form a precipitation hardening phase is the main means of strengthening, 17-4PH attenuation performance, anti-corrosion fatigue and anti-drop performance.

17-4PH stainless steel, is martensitic precipitation hardening stainless steel, equivalent to the Chinese brand: 0Cr17Ni4Cu4NB. Precipitation hardening section steel with 17-4PH added copper. 17-4PH for the manufacture of shaft, steam turbine components.

17-4 PH Proportion by mass (%)

CMnPSSiCrNiCuNb, Ta
0.07 max.1.0 max.0.04 max.0.03 max.1.0 max.15.0–17.53.0–5.03.0–5.00.15–0.45

Standards: AISI, ASTM

Grade: 17-4 PH(SUS630)

UNS number: S17400

17-4 PH alloy is composed of copper, niobium precipitation, hardening, martensitic stainless steel.
Features: After heat treatment, the mechanical properties of the product are improved and compressive strength up to 1100-1300 MPa (160-190 ksi) can be achieved. This grade can not be used at temperatures above 300°C (572°F) or very low temperatures. It has good corrosion resistance to atmospheric and dilute acids or salts, and its corrosion resistance is the same as 304 and 430.

17-4 PH is a martensitic precipitation hardened stainless steel .17-4 PH performance characteristics is easy to adjust the strength level, you can change the heat treatment process to be adjusted.Martensite transformation and aging treatment to form a precipitation hardening phase is the main means of strengthening, 17-4 PH attenuation performance, anti-corrosion fatigue and anti-drop performance.17-4 ph bar

Application areas

  • Offshore platforms, helicopter decks, other platforms food industry
  • Pulp and paper industry
  • Aerospace (turbine blades)
  • Mechanical components
  • Nuclear waste bin

17-4 PH alloy is precipitated, hardened, martensitic stainless steel.

The 17-4 PH alloy is a precipitated, hardened, martensitic stainless steel consisting of copper, niobium/columbium.

This grade has high strength, hardness (up to 300 C C / 572m2F) and corrosion resistance and other characteristics.

After heat treatment, the mechanical properties of the product are further improved and compressive strength up to 1100-1300 mpa (160-190 ksi) can be achieved.

This grade can not be used at temperatures above 300°C (572°F) or very low temperatures. It has good corrosion resistance to atmospheric and dilute acids or salts. Its corrosion resistance is the same as that of 304 and 430.

17-4 PH Mechanical properties

  • Tensile strength σb (MPa): 480°C aging, ≥ 1310; 550°C aging, ≥ 1060; 580°C aging, ≥ 1000; 620°C aging, ≥ 930
  • Conditions Yield strength σ0.2 (MPa): 480°C aging, ≥1180; 550°C aging, ≥1000; 580°C aging, ≥865; 620°C aging, ≥725
  • Elongation rate δ5 (%): 480°C aging, ≥10; 550°C aging, ≥12; 580°C aging, ≥13; 620°C aging, ≥16
  • Sectional shrinkage ψ (%): 480°C aging, ≥40; 550°C aging, ≥45; 580°C aging, ≥45; 620°C aging, ≥50
  • Hardness: solid solution ≤ 363HB and ≤ 38HRC; 480°C aging, ≥ 375HB and ≥ 40HRC; 550°C aging, ≥ 331HB and ≥ 35HRC; 580°C aging,
  • ≥ 302HB and ≥ 31HRC; 620°C aging, ≥ 277HB and ≥ 28HRC
  • Density: 7.80g / cm3

17-4 PH Heat treatment specification

  1. 1020 ~ 1060°C solid solution fast cooling
  2. 480°C aging, after solution treatment, 470 ~ 490°C air cooling
  3. 550°C aging, after solution treatment, 540 ~ 560°C air cooling
  4. 580°C aging, after solution treatment, 570 ~ 590°C air cooling
  5. 620°C aging, after solution treatment, 610 ~ 630°C air cooling

Metallography: