C72900 Introduction
Copper alloys are of many types. The addition of various other elements provides each alloy its distinct characteristics. The addition of nickel to a copper alloy improves strength and corrosion resistance. Copper nickel alloys are also called cupronickel alloys.
The following datasheet discusses the chemical composition and properties of copper UNS C72900.
Other Designations
Equivalent material to UNS C72900 copper alloy is ASTM B740.
제작
- 용접 – Soldering, seam welding, spot welding, butt welding, coated metal arc welding, brazing, gas shielded arc welding are all excellent methods. Oxyacetylene welding can also be used.
- 단조 – The hot forging temperature for copper UNS C72900 alloy ranges between 649 and 871°C (1200 and 1600°F).
- Hot working – Copper UNS C72900 alloy has good hot working abilities.
- 냉간 가공 – Copper UNS C72900 alloy has excellent cold working properties.
- 가열 냉각 – Copper UNS C72900 alloy is annealed at temperatures 824ºC (1515ºF).
화학적 구성 요소
The chemical composition of UNS C72900 copper alloy is outlined in the following table.
강요 | |||||||||
---|---|---|---|---|---|---|---|---|---|
와 함께(1,2) | 납(삼) | Sn | 아연 | 철 | Ni(4) | 마그네슘 | 미네소타 | NB | |
Min (%) | 7.5 | 14.5 | |||||||
Max (%) | 렘 | 0.02 | 8.5 | 0.50 | 0.50 | 15.5 | 0.15 | 0.30 | 0.10 |
(1) Cu + Sum of Named Elements 99.7% min. (2) Cu value includes Ag. (3) 0.005% Pb max. for hot rolling. (4) Ni value includes Co. |
Mechanical Properties *
형태 | 성질 | Temper Code | 인장 강도 (ksi) | YS-0.2% Offset (ksi) | YS-0.5% Ext (ksi) | YS-0.05% Offset | 연장 (%) |
---|---|---|---|---|---|---|---|
조각 | 1/2 Hard and Spinodal Hardened (1/2 TS) | TS02 | 145 Min for Standard | 125 Min for Standard | 3 Typ | ||
1/4 Hard and Spinodal Hardened (1/4 TS) | TS01 | 130 Min for Standard | 105 Min for Standard | 4 Typ | |||
3/4 Hard and Spinodal Hardened (3/4 TS) | TS03 | 155 Min for Standard | 135 Min for Standard | 2 Typ | |||
Hard and Spinodal Hardened | TS04 | 165 Min for Standard | 145 Min for Standard | 2 Typ | |||
Mill-hardened Temper, TM – 1/2 Hard | TM02 | 105 Min for Standard | 90 Min for Standard | 80 Min for Standard | 15 Typ | ||
Mill-hardened Temper, TM – 1/2 Hard | TM00 | 95 Min for Standard | 75 Min for Standard | 70 Min for Standard | 22 Typ | ||
Mill-hardened Temper, TM – Hard | TM04 | 115 Min for Standard | 105 Min for Standard | 95 Min for Standard | 10 Typ | ||
Mill-hardened Temper, TM – XHMS Spring | TM08 | 150 Min for Standard | 140 Min for Standard | 125 Min for Standard | 2 Typ | ||
Mill-hardened Temper, TM -XHM – Extra Hard | TM06 | 130 Min for Standard | 120 Min for Standard | 105 Min for Standard | 6 Typ | ||
Solution Heat Treated | TB00 | 64 Min for Standard | 24 Min for Standard | 32 Typ | |||
Solution Heat Treated and Cold Worked: 1/2 Hard | TD02 | 85 Min for Standard | 8 Typ | ||||
Solution Heat Treated and Cold Worked: 1/4 Hard | TD01 | 75 Min for Standard | 50 Min for Standard | 18 Typ | |||
Solution Heat Treated and Cold Worked: 3/4 Hard | TD03 | 95 Min for Standard | 80 Min for Standard | 3 Typ | |||
Solution Heat Treated and Cold Worked: Hard | TD04 | 100 Min for Standard | 85 Min for Standard | ||||
Spinodal Hardened-Low Strength (ATLS) | TX00 | 120 Min for Standard | 95 Min for Standard | 6 Typ | |||
* Measured at room temperature, 68°F (20°C). |
물리적 특성
Melting Point – Liquidus°F | 2039 |
---|---|
Melting Point – Solidus°F | 1742 |
Densitylb/cu in. at 68°F | 0.323 |
비중 | 8.94 |
Electrical Conductivity% IACS at 68°F | 7.8 (1) |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 17 |
Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.1 |
Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
Modulus of Elasticity in Tensionksi | 18500 |
Modulus of Rigidityksi | 7500 |
(1)Aged condition. |
제작 속성
기술 | 적당 |
---|---|
납땜 | 훌륭한 |
브레이징 | 훌륭한 |
옥시아세틸렌 용접 | 좋은 |
가스 차폐 아크 용접 | 훌륭한 |
코팅 금속 아크 용접 | 훌륭한 |
스폿 용접 | 훌륭한 |
솔기 용접 | 훌륭한 |
맞대기 용접 | 훌륭한 |
냉간 가공 능력 | 훌륭한 |
열간 성형 능력 | 좋은 |
일반적인 제조 공정
No fabrication process properties for this alloy
열적 특성
치료 | 최저한의* | 최고* | ||
---|---|---|---|---|
가열 냉각 | 1515 | |||
뜨거운 작동 온도 | 1200 | 1600 | ||
* 온도는 화씨로 측정됩니다. |
일반적인 용도
제품 카테고리 | 제품 | 사유 카테고리 | 이유 |
---|---|---|---|
전기 같은 | 커넥터 | 전도도(전기) | 전기 전도도 |
커넥터 | 전도도(열) | 열 전도성 | |
커넥터 | 내식성 | 내식성 | |
커넥터 | 내식성 | Resistant to Oxidation | |
커넥터 | 성형 특성 | 성형성 | |
커넥터 | 기계적 성질 | 높은 탄성 계수 | |
커넥터 | 기계적 성질 | 매우 높은 강도 | |
커넥터 | 열적 특성 | 스트레스 완화에 대한 저항 | |
콘택트 렌즈 | 전도도(전기) | 전기 전도도 | |
콘택트 렌즈 | 전도도(열) | 열 전도성 | |
콘택트 렌즈 | 내식성 | 내식성 | |
콘택트 렌즈 | 내식성 | Corrosion Resistance to Fresh Water | |
콘택트 렌즈 | 내식성 | Corrosion Resistance to Salt Water | |
콘택트 렌즈 | 내식성 | Resistant to Oxidation | |
콘택트 렌즈 | 성형 특성 | 성형성 | |
콘택트 렌즈 | 기계적 성질 | 높은 탄성 계수 | |
콘택트 렌즈 | 기계적 성질 | 매우 높은 강도 | |
콘택트 렌즈 | 열적 특성 | 스트레스 완화에 대한 저항 | |
Controls | 전도도(전기) | 전기 전도도 | |
Controls | 전도도(열) | 열 전도성 | |
Controls | 내식성 | 내식성 | |
Controls | 내식성 | Corrosion Resistance to Salt Water | |
Controls | 기계적 성질 | 고강도 | |
Miniaturized Sockets | 내식성 | 내식성 | |
Miniaturized Sockets | 성형 특성 | 성형성 | |
Miniaturized Sockets | 기계적 성질 | 높은 탄성 계수 | |
Miniaturized Sockets | 기계적 성질 | 매우 높은 강도 | |
Relay Elements | 전도도(전기) | 전기 전도도 | |
Relay Elements | 전도도(열) | 열 전도성 | |
Relay Elements | 내식성 | 내식성 | |
Relay Elements | 내식성 | Resistant to Oxidation | |
Relay Elements | 성형 특성 | 성형성 | |
Relay Elements | 기계적 성질 | 높은 탄성 계수 | |
Relay Elements | 기계적 성질 | 매우 높은 강도 | |
Relay Elements | 열적 특성 | 스트레스 완화에 대한 저항 | |
Switches | 전도도(전기) | 전기 전도도 | |
Switches | 전도도(열) | 열 전도성 | |
Switches | 내식성 | 내식성 | |
Switches | 내식성 | Corrosion Resistance to Salt Water | |
Switches | 기계적 성질 | 고강도 | |
산업 | 스프링스 | 내식성 | 내식성 |
스프링스 | 내식성 | Resistant to Oxidation | |
스프링스 | 성형 특성 | 성형성 | |
스프링스 | 기계적 성질 | 높은 탄성 계수 | |
스프링스 | 기계적 성질 | 매우 높은 강도 | |
스프링스 | 열적 특성 | 스트레스 완화에 대한 저항 | |
철사 | 내식성 | 내식성 | |
철사 | 내식성 | Resistant to Oxidation | |
철사 | 성형 특성 | 성형성 | |
철사 | 기계적 성질 | 높은 탄성 계수 | |
철사 | 기계적 성질 | 매우 높은 강도 | |
선박 | 해양 부품 | 내식성 | 내식성 |
해양 부품 | 내식성 | Corrosion Resistance to Fresh Water | |
해양 부품 | 내식성 | Corrosion Resistance to Salt Water | |
해양 부품 | 내식성 | Resistant to Oxidation | |
해양 부품 | 성형 특성 | 성형성 | |
해양 부품 | 기계적 성질 | 높은 탄성 계수 | |
해양 부품 | 기계적 성질 | 매우 높은 강도 | |
해양 부품 | 열적 특성 | 스트레스 완화에 대한 저항 |
적용 사양
형태 | 특정 하위 양식 | 애플리케이션 | 체계 | 기준 | 설명 |
---|---|---|---|---|---|
Rod & Bar | 천식 | B929 | COPPER-NICKEL-TIN SPINODAL ALLOY ROD AND BAR | ||
조각 | 천식 | B740 | STRIPS, COPPER-NICKEL-TIN SPINODAL ALLOY STRIP |