導入

Nickel Aluminum Bronze (NAB) tubes are critical components in marine and shipbuilding applications, offering exceptional resistance to seawater corrosion, cavitation, and biofouling. This guide focuses on three primary NAB alloys – C95800, C63200, and C95500 – and their specific applications in marine systems.

Marine System Requirements

Marine environments present unique challenges for tube materials:

  • Continuous exposure to seawater corrosion
  • High-pressure operating conditions
  • Temperature variations
  • Cavitation and erosion risks
  • Biofouling concerns
  • Compliance with marine standards (ASTM, Lloyd’s Register, DNV)

応用分野

1. Seawater Cooling Systems

Primary applications in marine cooling systems include:

  • Main engine cooling circuits
  • Auxiliary machinery cooling
  • Air conditioning systems
  • 熱交換器
  • Condensers
System ComponentRecommended AlloyAlternativeKey Selection Factors
Main Engine CoolingC95800C95500High erosion resistance, pressure rating
熱交換器C63200C95800Cost-effective, good heat transfer
Condenser TubesC95800C63200優れた耐食性
Auxiliary CoolingC63200C95500Balance of properties and cost

2. High-Pressure Systems

応用Operating Pressure (MPa)Recommended AlloyMinimum Wall Thickness (mm)
Hydraulic Lines20-30C955003.0
Fire Fighting15-25C958002.5
Ballast Systems10-15C632002.0
Test Pressure+50% of operatingAll gradesAs per class requirements

3. Performance Characteristics in Marine Environment

財産C95800C63200C95500Significance
Seawater Corrosion Rate (mm/year)0.0250.0250.025すべて優れています
Flow Velocity Max (m/s)15.212.213.7C95800スーペリア
生物付着耐性素晴らしいとても良い素晴らしいCritical for longevity
ガルバニック互換性素晴らしいとても良い素晴らしいWith hull materials

4. Dimensional Standards for Marine Applications

Nominal Size (mm)Wall Thickness (mm)Tolerance (mm)Standard Reference
15-501.5-2.5±0.15ASTM B466
50-1002.5-3.5±0.20ASTM B466
100-1503.5-5.0±0.25ASTM B466
150-3005.0-8.0±0.35ASTM B466

5. Installation and Maintenance Requirements

パラメータ仕様注意事項Standard Reference
Installation Temp-10°C to +40°CNormal conditionsClass requirements
Support Spacing20-40x ODBased on sizeISO 15749
Inspection Interval2-5 yearsBased on serviceIACS requirements
Service Life25+ yearsProper maintenanceDesign standard

6. Cost-Performance Analysis

要素C95800C63200C95500考慮
初期費用高い適度高いMaterial cost
設置費用標準標準標準Labor requirements
維持費低いLow-Medium低いLong-term reliability
ライフサイクルコスト素晴らしいとても良い素晴らしいTotal ownership cost

Selection Guidelines for Marine Systems

  1. Primary Cooling Systems
  • Use C95800 for critical main engine cooling
  • C63200 suitable for secondary cooling circuits
  • C95500 for high-pressure applications
  1. 熱交換器
  • C63200 for general service
  • C95800 for severe service conditions
  • C95500 for high-temperature applications
  1. Auxiliary Systems
  • C63200 for general service lines
  • C95800 for critical service areas
  • C95500 for high-stress applications

Quality Assurance Requirements

テストの種類要件頻度標準
化学分析Per grade specsEach heatASTM E478
Mechanical TestingAs specifiedPer lotASTM E8
Hydrostatic Test1.5x working pressure100%ASTM B466
NDTAs requiredPer specificationASTM E213

結論

For marine applications:

  • C95800: Best for critical seawater systems and main engine cooling
  • C63200: Economical choice for secondary systems
  • C95500: Optimal for high-pressure and high-temperature applications

Selection should consider:

  1. System criticality
  2. Operating conditions
  3. Life cycle costs
  4. Maintenance requirements
  5. Classification society requirements