The C95800 nickel aluminum bronze alloy follows strict compositional requirements as per ASTM B150/B150M standard:
要素
構成範囲(%)
銅
79.0 – 81.5
ニッケル(Ni)
4.0 – 5.0
アルミニウム(Al)
8.5~9.5
鉄(Fe)
3.5 – 4.5
マンガン(Mn)
0.8 – 1.5
シリコン(Si)
0最大.10
鉛(Pb)
0最大.03
2. 機械的性質
Standard mechanical properties at room temperature:
財産
価値
ユニット
抗張力
585-760
MPa
降伏強さ
245-485
MPa
伸長
15 (min)
%
硬度
160-190
Brinell
Impact Strength
34
Joules
密度
7.64
g/cm3
3. Standard Dimensions
Common available sizes for C95800 tubes:
Outer Diameter (mm)
Wall Thickness (mm)
Length (m)
15.88 - 25.4
1.65 – 3.38
3 – 6
31.75 - 50.8
2.11 – 4.78
3 – 6
63.5 – 101.6
3.18 – 6.35
3 – 6
114.3~219.1
4.78 – 12.7
3 – 6
273.0 – 406.4
6.35 – 19.1
3 – 6
4. 物性
財産
価値
ユニット
溶解範囲
1030-1060
℃
熱伝導率
42
W/m・K
電気抵抗率
13.3
μΩ・cm
熱膨張係数
16.2
μm/m・k
最高動作温度
315
℃
5. Key Applications
5.1 Marine Industry Applications
Propeller shaft sleeves
Pump housings
Valve bodies
Sea water piping systems
Marine hardware components
5.2 Oil & Gas Industry
Offshore platform components
海底機器
Pipeline fittings
ポンプのコンポーネント
Heat exchanger tubes
5.3 Chemical Processing
Chemical transport lines
Process equipment
Reaction vessels
Heat exchanger tubes
Distillation equipment
6. 耐食性
Performance ratings in various environments:
環境
Resistance Rating
注意事項
海水
素晴らしい
Superior resistance to chloride attack
淡水
素晴らしい
Low corrosion rates
工業的な雰囲気
とても良い
Forms protective oxide layer
Acids (mild)
良い
Depends on concentration
アルカリ
とても良い
Suitable for most alkaline environments
7. Manufacturing Standards
Applicable international standards:
標準
説明
ASTM B150/B150M
アルミニウム青銅の棒・棒・形材の標準規格
ASTM B171/B171M
Standard Specification for Copper-Alloy Plate and Sheet
ASTM B467
Standard Specification for Welded Copper-Nickel Pipe
MIL-C-24679
Military Specification for Copper-Nickel-Aluminum Bronze
8. Quality Testing Requirements
テストの種類
Method
頻度
化学分析
Spectrographic Analysis
ヒートごとに
Mechanical Testing
Tensile Test
ロットごと
Dimensional Check
Precision Measurement
100%
非破壊検査
超音波検査
必要に応じて
Hydrostatic Test
Pressure Testing
100%
9. Advantages and Benefits
Key benefits of C95800 tubes:
Superior corrosion resistance in marine environments
Excellent mechanical strength
優れた耐摩耗性
High impact strength
Superior fatigue resistance
良好な機械加工性
Excellent weldability
10. Storage and Handling
Storage recommendations:
側面
要件
温度
Room temperature
湿度
< 60% relative humidity
Storage Position
Horizontal on suitable racks
保護
Cover from dust and debris
Identification
Clear marking and tagging
11. Certifications Required
Common certification requirements:
証明書の種類
説明
Material Test Certificate (EN 10204 3.1)
Chemical and mechanical properties
Manufacturing Process Certificate
Production process details
Quality System Certificate
ISO 9001:2015 compliance
Non-destructive Test Reports
As per customer specification
Third-Party Inspection Reports
When required
12. Maintenance Recommendations
Maintenance Aspect
頻度
Action
目視検査
四半期
Check for surface defects
Thickness Measurement
毎年
超音波検査
クリーニング
As needed
Remove deposits
Corrosion Check
Semi-annually
Inspect critical areas
This comprehensive guide provides essential information for engineers, procurement professionals, and technical specialists working with C95800 nickel aluminum bronze tubes. For specific applications or requirements, please consult with qualified metallurgists or engineering professionals.