CharacteristicAluminum BronzeTin BronzeCompositionMain Alloying ElementAluminum (5-12%)Tin (5-25%)Other Common ElementsIron, Nickel, Manganese, SiliconPhosphorus, Lead, ZincTypical GradesC95200 (Cu-9Al-2Fe)C95400 (Cu-11Al-4Fe)C95500 (Cu-11Al-4Ni-4Fe)C90700 (Cu-10Sn)C93200 (Cu-7Sn-7Pb-2Zn)C52100 (Cu-8Sn-0.3P)Physical PropertiesColorGolden to reddish-goldReddish to pale yellowDensity7.7-8.1 g/cm³8.7-8.9 g/cm³Melting Point1030-1080°C (1886-1976°F)830-1000°C (1526-1832°F)Thermal Conductivity30-50 W/m·K50-70 W/m·KElectrical Conductivity10-18% IACS15-25% IACSMechanical PropertiesTensile Strength550-1200 MPa220-550 MPaHardness140-280 Brinell60-180 BrinellDuctility5-20% elongation10-30% elongationWear ResistanceExcellentGoodFatigue StrengthHigherGood, but lower than aluminum bronzeCorrosion ResistanceSeawater EnvironmentExcellentGood,...
Introduction to Aluminum Bronze Aluminum bronze is a family of copper-based alloys that primarily consists of copper alloyed with aluminum, often incorporating additional elements such as iron, nickel, manganese, and silicon. This versatile alloy combines the excellent corrosion resistance of bronze with the strength and lightness of aluminum, resulting in a material that offers a...
La produzione di flange in lega a base di nichel è un processo complesso e intricato, prevalentemente progettato per i sistemi di connessione dei tubi che operano a temperature elevate, elevate pressioni e ambienti corrosivi estremi. Il processo di produzione prevede più fasi, dalla selezione dei materiali all'ispezione finale, in cui ogni fase svolge un ruolo cruciale nel garantire le prestazioni e la qualità del ...
Le flange in lega a base di nichel sono componenti essenziali utilizzati in vari settori grazie alle loro proprietà superiori, come eccellente resistenza alla corrosione, capacità di gestione delle alte temperature ed eccezionale resistenza meccanica. Queste flange vengono impiegate in ambienti difficili dove altri materiali fallirebbero, garantendo l'affidabilità e la longevità delle installazioni in settori che vanno dall'aerospaziale alla lavorazione chimica....
Inconel C263 and Hastelloy C276 are both high-performance nickel-based superalloys, each with unique properties that make them valuable in different industrial applications. This comparison highlights the key differences between these two alloys, including their chemical composition, mechanical properties, temperature performance, and typical uses. Understanding these distinctions is crucial for engineers and designers when selecting materials...
Introduzione Le leghe di Inconel e Titanium sono materiali ad alte prestazioni cruciali nell'ingegneria moderna. Questo confronto esplora le loro caratteristiche chiave, tra cui composizione chimica, proprietà meccaniche, prestazioni di temperatura e applicazioni del settore. Esaminando questi aspetti, miriamo a fornire una guida completa per ingegneri e designer nella selezione dei materiali. Composizione chimica (esempio di leghe) Element Inconel 718 Titanium Grade ...
Nimonic 90 e Inconel 718 sono entrambe rinomate SuperAlloys a base di nichel che mostrano prestazioni eccezionali in condizioni estreme, rendendoli molto ricercati in varie applicazioni ad alto stress. Queste leghe sono specificamente progettate per fornire eccezionali proprietà meccaniche, resistenza all'ossidazione e maggiore durata in ambienti soggetti a temperature elevate e sostanze corrosive. La comprensione del loro ...
NIMONIC and INCONEL are highly regarded nickel-based superalloys commonly utilized across various industries for their exceptional performance characteristics. Key aspects of these alloys include: Composition Alloy Nickel (Ni) Chromium (Cr) Iron (Fe) Molybdenum (Mo) Cobalt (Co) Titanium (Ti) Aluminum (Al) NIMONIC 63-70% 15-20% Bal. 1-3% 8-11% 3-4% 0.2-0.5% INCONEL 58-72% 14-22% Bal. 2-10% 3-8% <1%...
Introduction NIMONIC 80A is a nickel-chromium-based superalloy known for its exceptional strength and oxidation resistance at high temperatures. This document explores the properties, applications, advantages, and industries utilizing NIMONIC 80A. Material Properties Composition The composition of NIMONIC 80A is crucial to its performance at high temperatures. The following table details its chemical composition: Element Percentage...