This article compares the characteristics of UNS C63200 and UNS C95800 copper alloys, detailing their chemical compositions, mechanical properties, performance at different temperatures, industry applications, shape, size, production standards, and additional relevant factors.
Composizione chimica
Elemento
C63200 (%)
C95800 (%)
Alluminio (Al)
8.7 – 9.5
8.5 – 9.5
Nichel (Ni)
4.0 – 4.8
4.0 – 5.0
Ferro (Fe)
3.5 – 4.3
3.5 – 4.5
Manganese (Mn)
1.2 – 2.0
0.8 – 1.5
Silicon (Si)
0.1
0.1
Piombo (Pb)
0.02
0.03
Rame
Equilibrio
79
Proprietà meccaniche
Proprietà
C63200
C95800
Durezza (Rockwell B)
85-95
85-90
Resistenza alla trazione
550MPa
620 MPa
Resa
300 MPa
380 MPa
Elongation at Break
10%
8%
Modulo elastico
117 GPa
117 GPa
Impatto Charpy
25.0 J
15.0 J
lavorabilità
70
40
Prestazioni a diverse temperature
Proprietà
C63200
C95800
Punto di fusione
1033°C (1911°F)
1060°C (1940°F)
Conduttività termica
50.0 W/mK (346 BTU in/hr.ft²°F)
40.0 W/mK (276 BTU in/hr.ft²°F)
Thermal Expansion Coefficient
16.3 µm/m°C
16.5 µm/m°C
Applicazioni industriali
Applicazione
C63200
C95800
Componenti marini
Yes
Yes
Pump and Valve Components
Yes
Yes
Electrical Connectors
Limitato
Limitato
Heavy Machinery Parts
Limitato
Yes
Forma e dimensione
Attribute
C63200
C95800
Available Shapes
Rods, Bars
Rods, Bars
Standard Sizes
Various
Various
Common Forms
Sheet, Plate
Sheet, Plate
Standard di produzione
Standard
C63200
C95800
ASMA
B505, B150
B505, B150
COME ME
SFA 5.7
SFA 5.7
SAE
J461, J463
J461, J463
Saldatura e lavorazione
Processing Method
C63200
C95800
Welding Compatibility
Good (with precautions)
Limitato
Preferred Welding Method
Gas shielded, resistance
Somewhat difficult
Lucidatura
Good polishing capability
Moderate polishing capability
Trattamento termico
Yes
Yes
Cold Processing
Moderate capacity
Limitato
Vantaggi e svantaggi
Attribute
C63200
C95800
Vantaggi
Good strength, corrosion resistant
Excellent wear resistance, high strength
Svantaggi
Lower wear resistance compared to C95800
Higher cost, lower machinability
Similar Products
Similar Products
Proprietà
Copper Nickel Alloys
Good corrosion resistance, suitable for marine applications.
Aluminium Bronze Alloys
High strength and corrosion resistance, often used in similar applications.
Comparison of Similar Products
Prodotto
Resistenza alla corrosione
Forza
Applicazioni
UNS C63200
Alto
Moderare
Marine, Pumps, Valves
UNS C95800
Più alto
Alto
Pumps, Heavy Machinery
Copper Nickel Alloys
Molto alto
Moderare
Marine, Plumbing
Conclusione
In conclusion, both UNS C63200 and UNS C95800 copper alloys exhibit unique properties that make them suitable for different applications. C63200 is characterized by its good strength and corrosion resistance, making it a reliable option for marine components. In contrast, C95800 provides superior wear resistance and is better suited for high-stress applications, particularly in heavy machinery. Understanding these distinctions will facilitate informed choices in material selection for various engineering requirements. If you have any further questions or need additional information, feel free to ask!
Per fornire le migliori esperienze, utilizziamo tecnologie come i cookie per archiviare e/o accedere alle informazioni del dispositivo. Il consenso a queste tecnologie ci consentirà di elaborare dati come il comportamento di navigazione o gli ID univoci su questo sito. Non acconsentire o revocare il consenso, può influire negativamente su alcune caratteristiche e funzioni.
Funzionale
Sempre attivo
L'archiviazione tecnica o l'accesso sono strettamente necessari al legittimo fine di consentire la fruizione di uno specifico servizio esplicitamente richiesto dall'abbonato o dall'utente, ovvero al solo fine di effettuare la trasmissione di una comunicazione su una rete di comunicazione elettronica.
Preferenze
L'archiviazione tecnica o l'accesso è necessario per il legittimo scopo di memorizzare le preferenze che non sono richieste dall'abbonato o dall'utente.
Statistiche
L'archiviazione tecnica o l'accesso utilizzato esclusivamente a fini statistici.L'archiviazione tecnica o l'accesso utilizzato esclusivamente per finalità statistiche anonime. Senza un mandato di comparizione, la conformità volontaria da parte del tuo provider di servizi Internet o registrazioni aggiuntive da parte di terzi, le informazioni memorizzate o recuperate solo a questo scopo non possono solitamente essere utilizzate per identificarti.
Marketing
La memorizzazione tecnica o l'accesso sono necessari per creare profili utente per l'invio di pubblicità o per tracciare l'utente su un sito Web o su più siti Web per scopi di marketing simili.