C70600 PIPE
The alloy has good corrosion resistance to clean contaminated seawater and is used extensively on heat exchangers using seawater in power plants, desalination, petrochemical plants, etc
Length : 500~15000MM
OD : 10-325 MM
WT : 1~25MM
C70600 white copper tube and other copper-nickel alloy tube products have excellent corrosion resistance and heat transfer performance, and can maintain good working condition in various harsh environments. Copper-nickel alloy pipes are made of pure material, with smooth surface and precise dimensions.
C70600 PROPERTIES
سبيكة | المنتج | لين، لطف، هدأ | Section size(mm) | الطول (مم)، الحد الأقصى. | |
من. | وزن. | ||||
BFe10-1-1 C70600 | Drawn pipes | M、Y2、Y | 10~160 | 1~8 | OD.≤50 L1000~7000OD.>50 L500~6000 |
BFe10-1.6-1 | Copper Nickeltubes and Pipes for Marine shipbuilding | م | 10~159 | 1.0~3.5 | 2000~6000 |
BFe10-1.6-1 | 10~194 | 1.0~3.5 | 6000 | ||
>194~325 | 3.0~5.5 | Negotiated | |||
BFe10-1-1、BFe10-1.6-1、C70600、7060X | 10~368 | 1.0~5.5 | 4000~6000 | ||
22-160 | 3-10 | ||||
BFe10-1-1 C70600 | Condenser andHeat Transfomerpipes | م | 10~160 | 1~4.5 | 500~6000 |
Y、Y2 | 10~76 | 1~4.5 | <15000 | ||
BFe10-1-1 | Extruded pipes | ص | 70~250 | 10~25 | 500~3000 |
C70600 、C7060X | C70600 、C7060X Negotiated |
C70600 Chemical Composition
سبيكة | درجة حرارة التقسية | ||||||||||||
مع | ني+Co | Fe | Mn | الرصاص | ص | س | ج | و | Zn | Sn | impurities | co | |
BFe10-1-1 | ريم | 9.0-11.0 | 1.0-1.5 | 0.5~1.0 | 0.02 | 0.006 | 0.01 | 0.05 | 0.15 | 0.3 | 0.03 | 0.7 | |
BFe10 -1.5 -1 | ريم | 10.0-11.0 | 1.0-2.0 | 0.50-1.0 | 0.01 | ― | 0.05 | 0.05 | 一 | ― | 一 | 0.6 | |
C7060 | ريم | 9.0-11.0 | 1.0-1.8 | 0.2-1.0 | 0.02 | 0.5 | |||||||
C70600 | ريم | 9.0-11.0 | 1.0-1.8 | 1.0 | 0.05 | 1.0 | |||||||
CuNil0FelMn | ريم | 9.0-11.0(Ni) | 1.0-2.0 | 0.50-1.0 | 0.02 | 0.02 | 0.05 | 0.05 | 0.5 | 0.03 | 0.2 | 0.1 |
لين، لطف، هدأ | Tensile Strength Rm/ (N/mm2) | Elongation A/ % min | HV | سمك 12-300 مم × عرض 200-2300 مم |
م | ≥290 | 30 | 75~110 | 70~105 |
Y2 | ≥310 | 12 | 105 | 100 |
ي | ≥480 | 8 | 150 | 145 |
C70600 FEATURES
Copper-nickel alloy is excellent in corrosion resistance, mainly used in desalination evaporator, central air conditioning condenser, ship air cooler, petrochemical cooler, power plant steam turbine condenser.
Drawn pipe/tube(big)

C70600 Drawn pipe/tube

C70600 Extruded pipe/tube

الاستخدامات النموذجية
Corrosion resistant parts and condensers, heat exchangers